Greetings!

I recently purchased a Heritage Limited Edition in REB. I had paint protection applied on the front (hood, front quarters, A-Pillar) and rockers. When the detailer was applying they noticed some galvanic corrosion. Advised to take it to the dealership and bring it to their attention. Said he has had this happen before and said the mfg usually reimburses/pays for the paint protection film to be re-applied (if needed)

Now, not everything that has paint protection has this issue but it does run on the rockers and some parts of the hood and door.

I brought it to the dealership about a month ago and they said it needed to be repaired and also said that Ford should pay for any of the paint protection that needed to be replaced.

I dropped it off yesterday and brought up the paint protection again and was told that they would have to get the service manager who wouldn’t be back until Monday.

Received call today that they will not reimburse for any paint protection to be re-applied.

Has anyone ran across this before? Do I eat the cost? Bring it to the service manager’s attention? Go to Ford?

Not sure what is “normal” or what the expectation should be.

Thanks for the advice!
Sponsored

 
OP
OP
origiNOLE

origiNOLE

Heritage
Member
Joined
Sep 3, 2023
Threads
3
Messages
24
Reaction score
17
Location
Huntsville, AL
Vehicle(s)
2017 GS Corvette, 2023 Heritage Limited Edition
Your Bronco Model
Heritage
Clubs
 
Sorry, I should have took some photos. The dealership was taken them when I went but seemed kind of hard to photograph. I will see if the dude who took them still has them and then see if he can send my way.

Definitely on that portion below the door kind of the lip. There were several areas. Buddy at work said Jeeps had these problems too.
 

KABQ

Base
Well-Known Member
First Name
Aaron
Joined
Aug 16, 2021
Threads
17
Messages
2,468
Reaction score
7,730
Location
Albuquerque, NM
Vehicle(s)
'93 4Runner, '84 Vanagon, '93 Miata, '14 LittleGuy
Your Bronco Model
Base
Clubs
 
Are you sure they used the right term? Galvanic corrosion specifically refers to dissimilar metals creating an anode-cathode system that causes corrosion due to different electrode potentials. Are you seeing the corrosion around steel bolts in aluminum?
 

2023bronco

Well-Known Member
Joined
Dec 19, 2022
Threads
19
Messages
1,017
Reaction score
2,314
Location
location
Vehicle(s)
vehicles
Your Bronco Model
Undecided
Yeah, I'm confused by all this. I'm wondering if it's just trash in the paint, which is found all over these Broncos. Definitely need pics.
 
OP
OP
origiNOLE

origiNOLE

Heritage
Member
Joined
Sep 3, 2023
Threads
3
Messages
24
Reaction score
17
Location
Huntsville, AL
Vehicle(s)
2017 GS Corvette, 2023 Heritage Limited Edition
Your Bronco Model
Heritage
Clubs
 
This was the term that I was informed of. Heck, I never heard of the term before. Could have been trash I guess. Some of the areas that was painted over was bumpy or rough. Barnacle like I guess. Painted over of course.